STEEL INDUSTRY
Mn is required in all grades of steel to act as deoxidiser or desulphuriser. Electrolytic Mn is added directly to the ladle in the final composition correction step. Producers of low carbon, HSLA or high Mn steels prefer the low levels of C, S, P, Si and H impurities in MMC’s products. The thicker flake and lower dust content of MMC’s LH flake improve material handling and increase Mn yield.